The data show the number of cycles to failure of samples of worsted yarn under cycles of repeated loading. There are three experimental conditions arranged in a 3 x 3 x 3 factorial design.
WoolData frame with 27 observations on the following 4 variables
x1length of test specimen (-1, 250 mm; 0, 300 mm; 1, 350 mm)
x2amplitude of loading cycle (-1, 8 mm; 0, 9 mm; 1, 10 mm)
x3load (-1, 40 g; 0, 45 g; 1, 50 g)
ycycles to failure