Fatigue: Cracks caused by metal fatigue
Description
The Fatigue
data frame has 262 rows and 3 columns.Format
This data frame contains the following columns:
- Path
-
an ordered factor with levels
1
< 2
< 3
< 4
< 5
<
6
< 7
< 8
< 9
< 10
<
11
< 12
< 13
< 14
< 15
<
16
< 17
< 18
< 19
< 20
<
21
giving the test path (or test unit) number. The
order is in terms of increasing failure time or decreasing
terminal crack length.
- cycles
-
number of test cycles at which the measurement is made
(millions of cycles).
- relLength
-
relative crack length (dimensionless).
Details
These data are given in Lu and Meeker (1993) where they state
``We obtained the data in Table 1 visually from figure 4.5.2 on page 242
of Bogdanoff and Kozin (1985).''
The data represent the growth of cracks in metal for 21 test units.
An initial notch of length 0.90 inches was made on each unit which then
was subjected to several thousand test cycles. After every 10,000
test cycles the crack length was measured. Testing was stopped if the
crack length exceeded 1.60 inches, defined as a failure, or at 120,000
cycles.